0cr23al5 Resistance Heating Flat Wire na may ISO9001 Certificate
Kable ng Resistance na gawa sa Nickel Chrome Alloys, Nickel Chrome Iron Alloys, Iron Chrome Aluminum Alloys, Copper Nickel Alloys.
Pangunahing ginagamit sa pampainit, elemento ng pag-init at resistor, atbp.
NiCr 80/20, NiCr 70/30, NiCr 60/15, NiCr 35/20
FeCrAl15-5, FeCrAl20-5, FeCrAl 25-5, atbp…
Constantan, Alloy 30, Alloy 60, Alloy 90, atbp.
Resistivity ng Elektrisidad mula 0.02 u ohm/m-1.53 u ohm/m
Temperatura ng Operasyon mula 200 C hanggang 1400 C
Pls maging maatubiling makipag-ugnayan sa amin kung mayroong anumang katanungan.
NiCr:
RESISTOHM 20, RESISTOHM 30, RESISTOHM 40, RESISTOHM 60, RESISTOHM 70, RESISTOHM 80
FeCrAl:
RESISTOHM 125, RESISTOHM 135, RESISTOHM 140,
RESISTOHM 145, RESISTOHM 153
CuNi
Constantan, Cuprothal 5, Cuprothal 10, Cuprothal 15, Cuprothal 30, Eurica
| Grado ng FeCrAl Alloy | Komposisyong Kemikal % | |||||||||
| C | P | S | Mn | Si | Cr | Ni | Al | Fe | Re | Iba pa |
| pinakamataas (≤) | ||||||||||
| 1Cr13Al4 | 0.12 | 0.025 | 0.025 | 0.7 | ≤1.00 | 12.5-15.0 | —- | 3.5-4.5 | 0.1 | Bal. |
| 0Cr15Al5 | 0.12 | 0.025 | 0.025 | 0.7 | ≤1.00 | 14.5-15.5 | —- | 4.5-5.3 | 0.1 | Bal. |
| 0Cr25Al5 | 0.06 | 0.025 | 0.025 | 0.7 | ≤0.60 | 23.0-26.0 | ≤0.60 | 4.5-6.5 | 0.1 | Bal. |
| 0Cr23Al5 | 0.06 | 0.025 | 0.025 | 0.7 | ≤0.60 | 20.5-23.5 | ≤0.60 | 4.2-5.3 | 0.1 | Bal. |
| 0Cr21Al6 | 0.06 | 0.025 | 0.025 | 0.7 | ≤1.00 | 19.0-22.0 | ≤0.60 | 5.0-7.0 | 0.1 | Bal. |
| 0Cr21Al4 | 0.06 | 0.025 | 0.025 | 0.7 | ≤1.00 | 21.0-23.0 | ≤0.60 | 3.0-5.2 | 0.1 | Bal. |
| 0Cr21Al6Nb | 0.05 | 0.025 | 0.025 | 0.7 | ≤0.60 | 21.0-23.0 | ≤0.60 | 5.0-7.0 | 0.1 | Bal. |
| 0Cr27Al7Mo2 | 0.05 | 0.025 | 0.025 | 0.7 | ≤0.40 | 26.5-27.8 | ≤0.60 | 6.0-7.0 | 0.1 | Bal. |
![]()
![]()
![]()
![]()
Komposisyon at Katangian ng Kemikal:
| Mga Ari-arian/Grado | NiCr 80/20 | NiCr 70/30 | NiCr 60/15 | NiCr 35/20 | NiCr 30/20 | |
| Pangunahing Kemikal Komposisyon (%) | Ni | Bal. | Bal. | 55.0-61.0 | 34.0-37.0 | 30.0-34.0 |
| Cr | 20.0-23.0 | 28.0-31.0 | 15.0-18.0 | 18.0-21.0 | 18.0-21.0 | |
| Fe | ≤ 1.0 | ≤ 1.0 | Bal. | Bal. | Bal. | |
| Pinakamataas na Paggawa Temperatura (ºC) | 1200 | 1250 | 1150 | 1100 | 1100 | |
| Resistivity sa 20ºC (μΩ · m) | 1.09 | 1.18 | 1.12 | 1.04 | 1.04 | |
| Densidad (g/cm3) | 8.4 | 8.1 | 8.2 | 7.9 | 7.9 | |
| Konduktibidad ng Termal (KJ/m· h· ºC) | 60.3 | 45.2 | 45.2 | 43.8 | 43.8 | |
| Koepisyent ng Thermal Pagpapalawak (α × 10-6/ºC) | 18 | 17 | 17 | 19 | 19 | |
| Punto ng Pagkatunaw (ºC) | 1400 | 1380 | 1390 | 1390 | 1390 | |
| Pagpahaba (%) | > 20 | > 20 | > 20 | > 20 | > 20 | |
| Istrukturang Mikrograpiko | austenite | austenite | austenite | austenite | austenite | |
| Magnetikong Katangian | hindi magnetiko | hindi magnetiko | hindi magnetiko | hindi magnetiko | hindi magnetiko | |
![]()
![]()
![]()
![]()
| Baitang ng CuNi Alloys | Resistivity ng kuryente (20 digriΩ mm² /m) | koepisyent ng temperatura ng resistensya (10^6/degree) | Densidad g/mm² | Pinakamataas na temperatura (antas) | Punto ng pagkatunaw (antas) |
| CuNi1 | 0.03 | < 1000 | 8.9 | 200 | 1085 |
| CuNi2 | 0.05 | < 1200 | 8.9 | 200 | 1090 |
| CuNi6 | 0.10 | < 600 | 8.9 | 220 | 1095 |
| CuNi8 | 0.12 | < 570 | 8.9 | 250 | 1097 |
| CuNi10 | 0.15 | < 500 | 8.9 | 250 | 1100 |
| CuNi14 | 0.20 | < 380 | 8.9 | 300 | 1115 |
| CuNi19 | 0.25 | < 250 | 8.9 | 300 | 1135 |
| CuNi22 | 0.30 | < 160 | 8.9 | 300 | 1150 |
| CuNi30 | 0.35 | < 100 | 8.9 | 350 | 1170 |
| CuNi34 | 0.40 | -0 | 8.9 | 350 | 1180 |
| CuNi40 | 0.48 | ± 40 | 8.9 | 400 | 1280 |
| CuNi44 | 0.50 | < -6 | 8.9 | 400 | 1280 |
![]()
![]()
![]()
![]()