Maligayang pagdating sa aming mga website!

Paggawa ng Mataas na Purty 99.6% Ni200 Ni201 Ni212 Pure Nickel N4 N6 Precision Stranded Alloy Wire para sa Makinarya ng Power Tools

Maikling Paglalarawan:


  • Model no.:Ni200 , Ni201 , Ni212
  • Density:8.9 g/cm3
  • ibabaw:maliwanag
  • package:SPOOL+ CARTON+ KASO
  • Trademark:Tankii
  • Pinagmulan:Shanghai China
  • Spool:DIN250, DIN200
  • Hs code:75052200
  • Detalye ng produkto

    FAQ

    Mga tag ng produkto

     

    Grade grade Ni+co Cu Si Mn C Cr S Fe Mg
    Ni201 Bal. .25 .3 .35 .02 .2 .01 .3 -
    Ni200 Bal. .25 .3 .35 .15 .2 .01 .3 -

     

    Alloy

    Standard Strand Construction, mm

    Paglaban, ω/m

    Strand diameter nominal, mm

    Metro bawat kilo

    NICR 80/20

    18 × 0.544+1 × 0.574

    0.252-0.278

    2.67

    26

    NICR 80/20

    19 × 0.61

    0.205-0.250

    3.05

     

    NICR 80/20

    18 × 0.523+1 × 0.574

    0.271-0.299

    2.67

    30

    NICR 80/20

    19 × 0.574

    0.227-0.251

    2.87

    25

    NICR 80/20

    36 × 0.385+1 × 0.45

    0.265-0.293

    2.76

    26

    NICR 60/15

    19 × 0.508

    0.286-0.318

    2.54

     

    NICR 60/15

    18 × 0.523+1 × 0.574

    0.276-0.305

    2.76

    30

    Ni200/Ni201

    19 × 0.574

    0.019-0.021

    2.87

    21

     

     

    N6 Chromel C, NI 60, N6, Hai-NICR 60, Tophet C, Residohm 60, Cronifer II,
    Electroloy, Nichrome, Alloy C, Ni 6, MWS-675, Stablohm 675
    N7 Ni 70, Chromel 70/30, N7, Hytemco, Hai-NICR 70, Balco, Tophet 30,
    Residtohm 70, Cronix 70, Stablohm 710
    N8 Chromel A, Ni 80, N8, Nichrome V, Hai-NICR 80, Tophet A, Residohm
    80, Cronix 80, Protoloy, Ni 8, Alloy A, MWS-650, Stablohm 650

     

     

    Mga Katangian/Baitang CR20NI80 CR30NI70 CR15NI60 CR20NI35 CR20NI30
    Pangunahing komposisyon ng kemikal Ni Pahinga Pahinga 55.0-61.0 34.0-37.0 30.0-34.0
      Cr 20.0-23.0 28.0-31.0 15.0-18.0 18.0-21.0 18.0-21.0
      Fe ≤ 1.0 ≤ 1.0 Pahinga Pahinga Pahinga
    Max. Patuloy na Serbisyo Temp. ng elemento 1200 1250 1150 1100 1100
    Resistivity sa 20oC (μ ω · m) 1.09 1.18 1.12 1.04 1.04
    Density (g/cm3) 8.4 8.1 8.2 7.9 7.9
    Thermal conductivity (kj/m · h · oc) 60.3 45.2 45.2 43.8 43.8
    Koepisyent ng pagpapalawak ng mga linya (α × 10-6/oc) 18 17 17 19 19
    Natutunaw na punto (tinatayang.) (OC) 1400 1380 1390 1390 1390
    Pagpahaba sa pagkalagot (%) > 20 > 20 > 20 > 20 > 20
    Istraktura ng mikrograpya Austenite Austenite Austenite Austenite Austenite
    Magnetic Properties nonmagnetic nonmagnetic nonmagnetic nonmagnetic nonmagnetic

     

     

     

     

     

     

     

     

     


  • Nakaraan:
  • Susunod:

  • Isulat ang iyong mensahe dito at ipadala ito sa amin