Komposisyon ng kemikal
Grade | Ni% | Cu% | Al% | Ti% | Fe% | Mn% | S% | C% | Si% |
Monel K500 | Min 63 | 27.0-33.0 | 2.30-3.15 | 0.35-0.85 | Max 2.0 | Max 1.5 | Max 0.01 | Max 0.25 | Max 0.5 |
Mga pagtutukoy
Form | Pamantayan |
Monel K-500 | UNS N05500 |
Bar | ASTM B865 |
Kawad | AMS4676 |
Sheet/Plate | ASTM B865 |
Pagpapanday | ASTM B564 |
Weld Wire | ERNiCu-7 |
Mga Katangiang Pisikal(20°C)
Grade | Densidad | Punto ng Pagkatunaw | Resistivity ng Elektrisidad | Mean Coefficient ng Thermal Expansion | Thermal Conductivity | Tukoy na init |
Monel K500 | 8.55g/cm3 | 1315°C-1350°C | 0.615 μΩ•m | 13.7(100°C) a/10-6°C-1 | 19.4(100°C) λ/(W/m•°C) | 418 J/kg•°C |
Mga Katangiang Mekanikal(20°C Min)
Monel K-500 | Lakas ng makunat | Lakas ng Yield RP0.2% | Pagpahaba A5% |
Annealed&Aged | Min. 896 MPa | Min. 586MPa | 30-20 |
Nakaraan: Paggawa ng Enamelled Copper Wire CuNi6 para sa Car/Auto Seat Heating Mat Susunod: 20 AWG Enameled Welding Tinned Copper Wire para sa Resistor Lead